Here we describe the evolution of iron-bearing phases in the firing of carbonate-rich illite and chlorite clay. Breakdown of chlorite forms an amorphous phase, which continues to retain iron in a (distorted) paramagnetic octahedral Site, until carbonates start to decompose and react at 750 degrees C, forming Ca-silicates. Only at this temperature can hematite nucleate and grow in specific micro-domains located in former chlorite flakes. At 950 degrees C, decomposition of Mite in the presence of an amorphous phase and CaO produces a melt in which nano-sized hematite may nucleate, although its growth is inhibited due to low diffusion with respect to soaking time.

Hematite nucleation and growth in the firing of carbonate-rich clay for pottery production

NODARI, LUCA;MARCUZZI, ENRICO;MARITAN, LARA;MAZZOLI, CLAUDIO;
2007

Abstract

Here we describe the evolution of iron-bearing phases in the firing of carbonate-rich illite and chlorite clay. Breakdown of chlorite forms an amorphous phase, which continues to retain iron in a (distorted) paramagnetic octahedral Site, until carbonates start to decompose and react at 750 degrees C, forming Ca-silicates. Only at this temperature can hematite nucleate and grow in specific micro-domains located in former chlorite flakes. At 950 degrees C, decomposition of Mite in the presence of an amorphous phase and CaO produces a melt in which nano-sized hematite may nucleate, although its growth is inhibited due to low diffusion with respect to soaking time.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11577/2447870
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 175
  • ???jsp.display-item.citation.isi??? 169
  • OpenAlex ND
social impact